面向光电路由平台的全互连芯片到晶圆混合铜键合工艺

Fully Interconnected Die-to-Wafer Hybrid Copper Bonding Pro- cess for Opto-Electrical Routing Platforms Da In Song, Byung-Ju Min, JungHo Cha, Seok-Geun Ahn, Sungbong Park, Shin Kwon, Yong-Jae Kim, Kwangil Shin, Woong Huh, Hyunjin Lee, Jaewon Hwang, Dong Su Yoo, Yunseo Lee, Han-Hy-
光子集成与工艺晶圆级测试与工艺波导/光栅/耦合器硅光/光子集成CPO共封装硅光3D/2.5D封装实验
ECOC 2026Samsung
实现光电同步混合键合,耦合损耗0.32dB

基本信息

作者
oung Kim, Jihyun Seo, Hyerin Kim, Jongmin Chung, Hyun-Chul Jung, and Kimin Jun(1)
机构
Samsung
会议
ECOC 2026(European Conference on Optical Communication)

摘要

我们展示了在晶粒到晶圆(die-to-wafer)混合键合系统上同时实现光电互连。即使光学层与电学层之间存在图形密度失配,CMP 侵蚀仍小于 100 Å。测得的倏逝耦合器损耗在 1310 nm 处为 0.32 dB,测得的电阻为 0.30 Ω。

Abstract

We demonstrate simultaneous opto-electrical interconnection on a die-to-wafer hybrid bonding system. CMP erosion is < 100 Å even with pattern density mismatch between optic and electric layers. Measured evanescent coupler loss is 0.32 dB at 1310 nm and measured electrical resistance is 0.30 Ω.

关键技术指标

指标数值说明
集成架构Die-to-Wafer 混合铜键合面向全互连光电路由平台,同时实现光电互连
互连类型光电同时互连光学层与电学层通过混合键合集成
CMP 侵蚀<100 Å光学层与电学层存在图形密度失配条件下
倏逝耦合器损耗0.32 dB@1310 nm
互连电阻0.30 Ω测得电学电阻

性能概述

CMP侵蚀<100Å;1310nm倏逝波耦合损耗0.32dB;电学电阻0.30Ω

技术路线

光互连、数据中心互连

应用场景

光电共封装、片上光互连