我们首次在超宽禁带、高K、晶体AlBN势垒GaN高电子迁移率晶体管(FerroHEMT)中观测到铁电栅控效应,所用的铁电氮化物势垒是迄今最薄的。我们观测到栅长从Lg = 1.5 µm 缩小到 44 nm 对AlBN/GaN FerroHEMT铁电栅控性能的强烈影响。短栅长Lg = 44 nm的器件表现出铁电栅控特性,具有大且可重复的Id-Vgs回滞环以及40 mV/decade的亚玻尔兹曼特性;而Lg = 800 nm至1.5 µm的较长栅长器件则几乎无回滞。我们报道了AlBN/GaN HEMT首个射频性能,fT/fMAX = 76/139 GHz,首次将外延超宽禁带、高K、铁电AlBN势垒技术引入射频与毫米波电子领域。
We report the first observation of ferroelectric gating in ultrawide bandgap, high-K, crystalline AlBN barrier GaN high electron mobility transistors (FerroHEMTs) using the thinnest ferroelectric nitride barrier to date. We observe a strong effect of gate length scaling from Lg = 1.5 µm to 44 nm on the ferroelectric gating performance of AlBN/GaN FerroHEMTs. While the short Lg = 44 nm gate length devices exhibit ferroelectric gating with large repeatable hysteretic Id-Vgs loops and 40 mV/decade sub-Boltzmann characteristic, the devices with longer Lg = 800 nm to 1.5 µm exhibit little to no hysteresis. We report the first RF performance of AlBN/GaN HEMTs with fT/fMAX = 76/139 GHz, introducing first epitaxial ultrawide bandgap, high-K, and ferroelectric AlBN barrier technology to RF and mm-wave electronics.
| 指标 | 数值 | 说明 |
|---|---|---|
| 截止频率/最高振荡频率 fT/fMAX | 76/139 GHz | AlBN/GaN HEMT首个射频性能,Lg ≈ 44 nm |
| 亚玻尔兹曼亚阈值斜率 | 40.5 mV/decade | Vds = 1 V下off→on扫描所得,低于60 mV/dec极限,指示铁电栅控 |
| 开态电流密度 Ion | 580 mA/mm | Lg ≈ 44 nm、Lsd = 600 nm、Wg = 50 µm器件在Vgs = 2 V下 |
| 开态电阻 Ron | 3.41 Ω·mm | Vgs = 2 V时;Vgs = 0 V时为9.5 Ω·mm |
| 峰值跨导 gm | 272 mS/mm | 44 nm栅长器件的峰值跨导 |
| AlBN相对介电常数 εr | 16.2(Al0.93B0.07N),AlN为8.8 | 由MIS电容C-V提取,约为AlN的两倍 |
| 栅压回滞窗口 ΔVg_hys | 3.1-3.9 V | 对应4 nm势垒与矫顽场|Ec| ≈ 4.375 MV/cm |
fT/fMAX = 76/139 GHz;亚玻尔兹曼摆幅 40.5 mV/decade
外延生长、铁电极化、高k金属栅
射频与毫米波电子、通信功率放大器