WaytoICT › 香农学术库 › IEDM 2025 › 论文

400 °C BEOL后道形成气体退火(FGA)致密化过程中掺杂In2O3薄膜晶体管的缺陷动力学与BTI实验与建模研究

Experiments and Modeling of Defect Dynamics and BTI in Doped In2O3 TFTs Undergoing Densification during 400 °C Post-BEOL Forming Gas Annealing (FGA)
新型沟道与材料器件氧化物半导体FET薄膜晶体管(TFT)互连/BEOL氧化物半导体(IGZO/ITO)实验+仿真
IEDM 2025Georgia Institute of Technology
首次用实验与DFT-MD揭示400°C FGA下In2O3 TFT氢缺陷两阶段演化及BTI极性反转,SS改善约37%。

基本信息

作者
Y.-H. Kuo1, C. Zhang1, P. G. Ravikumar1, S. Kang1, T. Song1, M. A. Villena2, L. Larcher3, H. Kim4, M. Hong4, P. Yun4, G. Thareja3, S. Yu1, D. Ha4, S. Datta1,6, J. E. Medvedeva5 and A. I. Khan1,6
机构
Georgia Institute of Technology
国家
美国
会议
IEDM 2025(International Electron Devices Meeting)
工艺节点
未提及(长沟道器件 Lch = 1 μm)
供电电压
过驱动电压 Vov = +1.5 V(BTI 应力条件)
工作温度
400 °C FGA 退火;BTI 应力测试温度 85 °C
电路架构
未提及(单器件底栅长沟道 TFT)

摘要

我们首次通过实验研究与基于DFT的液体淬火分子动力学(MD)模拟相结合,报道了工艺中必不可少的400 °C氢基BEOL后道退火(即FGA)对氧化物沟道TFT电学特性与BTI行为的影响,以及相应的形貌与缺陷演化。作为模型体系,我们选择了3.7 nm厚、4% W掺杂的In2O3沟道TFT,其栅氧为5 nm等离子体ALD生长的HfO2,并由3 nm Al2O3 / 3 nm HfO2混合叠层封装,可有效阻挡外来氢。主要发现为:(1) FGA早期致密化阶段(10 min)会产生浅能级/去局域化的In–H–In缺陷态(约位于费米能级以下0.65 eV),导致PBTI退化(从原始态的-27.45 mV退化到85 °C、Vov=+1.5V条件下2 ks应力后的−122 mV),并引入明显的IDS–VGS“Kink”;(2) 长时间退火(>40 min)因部分晶化而触发恢复:先前存在的H被俘获在深能级/局域化缺陷态中(In–OH诱导的In–In),限制了H的迁移,使PBTI恢复到较低水平(−10.4 mV)并消除“Kink”;(3) 总体上,60 min FGA使SS变陡约37%,同时改善PBTI与NBTI并伴随极性符号变化。这些结果阐明了关键的后道FGA过程中氢缺陷的动力学行为,并凸显了在不牺牲性能与可靠性的前提下,氢阻挡封装对氧化物沟道TFT的BEOL集成的重要性。

Abstract

We report, for the first time, the impact of essential, process-driven 400 °C hydrogen (H)-based post-BEOL annealing (i.e., FGA) on the electrical characteristics and BTI behavior of oxide channel TFTs, along with the associated morphological and defect evolution, through a combined experimental study and DFT-based liquid-quench molecular dynamics (MD) simulations. As a model system, we choose 3.7 nm thick 4 % W-doped In2O3-channel TFTs with a 5 nm plasma-ALD-grown HfO2 gate oxide, encapsulated by a 3 nm Al2O3 / 3 nm HfO2 hybrid layer that effectively blocks incoming hydrogen. The key findings are: (1) Early-stage densification during FGA (10 min) generates shallow-/delocalized In–H–In defect states (~0.65 eV below Fermi level), causing PBTI degradation (from -27.45 mV in the pristine state to −122 mV under 2 ks stressing at 85 °C, Vov=+1.5V) and introducing a distinct IDS–VGS "kink"; (2) Prolonged annealing (>40 min) triggers a recovery due to partial crystallization, trapping pre-existing H in deep/localized defect states (In–OH-induced In–In), limiting H mobility, restoring low PBTI (−10.4 mV) and erasing the "Kink"; (3) Overall, a 60 min FGA steepens SS by ~37%, improves both PBTI and NBTI with an associated sign change. These results elucidate H-defect dynamics during critical post-BEOL FGA and underscore the importance of hydrogen-blocking encapsulations for BEOL integration of oxide-channel TFTs without sacrificing performance and reliability.

关键技术指标

指标数值说明
亚阈值摆幅(SS)改善约 37%400 °C FGA 60 min 后 SS 变陡约 37%,表明界面陷阱密度降低
PBTI ΔVTH(10 min FGA)−122 mV85 °C、Vov=+1.5 V、2 ks 应力下,由原始态 −27.45 mV 退化而来
PBTI ΔVTH(60 min FGA)−10.4 mV长时间退火部分晶化后 H 被深能级俘获,PBTI 恢复至低漂移
氢致缺陷能级约 0.65 eV(费米能级以下)早期 FGA 形成的浅/去局域 In–H–In 施主态,诱发 Kink 与 PBTI 退化
沟道与栅介质厚度3.7 nm IWO / 5 nm HfO2 / 3 nm Al2O3 + 3 nm HfO2PE-ALD 250 °C 沉积的 W 掺杂 In2O3 沟道与混合氢阻挡封装叠层

性能概述

60 min FGA 后 SS 改善约 37%;PBTI 的 ΔVTH 由 10 min 的 −122 mV 恢复到 60 min 的 −10.4 mV

技术路线

BTI、电荷俘获、原子层沉积(ALD)、退火优化

应用场景

单片3D集成、BEOL后道氧化物TFT、先进逻辑

打开交互版 · AI 解读 / 同类对比 / 完整指标在香农学术库中查看(需会员)

同领域论文

← 返回香农学术库
蜀ICP备2020035321号-2