WaytoICT › 香农学术库 › IEDM 2025 › 论文

面向176层3D NAND闪存的高度可扩展隔离电荷陷阱氮化物层及其优异阈值电压分布与电荷保持特性

A Highly Scalable Isolated Charge Trap Nitride Layer Implemented in a 176-layer 3D NAND Flash with Superior Threshold Voltage Distribution and Charge Retention
存储器技术3D NAND3D NAND硅基CMOS氮化硅(SiN)实验+仿真
IEDM 2025SK hynix
在176层3D NAND中首次用沉积侧壁口袋隔离电荷陷阱氮化物,读取时间降11%、Vth分布收窄6.9%、高温保持提升45%。

基本信息

作者
Sang-wan Jin, Doyoung Kim, Seonghee Kim, Eunmi Kwon, Keonsoo Shim, Hyungjun Yang, Jongung Baek, Jeongah Hong, Yousang Yoon, Seokmin Jeon, Seongman Jeon, Sangseob Lee, Joon Hyuk Park, Ju Yeab Lee, Sanghyun Oh, Jum Soo Kim, Youngmann Cho, Seonyong Cha
机构
SK hynix
国家
韩国
会议
IEDM 2025(International Electron Devices Meeting)
工艺节点
176层 3D NAND(层间距缩小至电学极限)

摘要

本文首次在176层量产级3D NAND器件中成功实现了新型电荷陷阱氮化物隔离(CTI)技术。在该方案中,电荷陷阱氮化物(CTN)层被通过沉积工艺形成侧壁的口袋结构所限制,这是首次实现,从而提升了CTI的可扩展性。我们达到了足够的工艺成熟度,可在较大晶圆面积上制造功能完整的芯片,从而实现芯片级的阈值电压(Vth)分布与保持特性评估。与传统连续CTN单元相比,该技术使读取时间(tR)缩短11%,Vth分布宽度收窄6.9%,循环后的高温保持特性提升45%。这些结果表明,从Vth分布角度看,当前的层间距(tier pitch)极限可再缩小4 nm;从保持特性角度看,可再缩小10 nm以上,从而支持我们的CTI技术成为持续推进3D NAND微缩的有力方案。

Abstract

In this work, we present the successful implementation of a novel charge trap nitride isolation (CTI) technology in a 176-layer production-scale 3D NAND device. In this approach, the charge trap nitride (CTN) layer is confined by a pocket with sidewalls formed through a deposition process, a first-time implementation that improves CTI scalability. We achieved sufficient process maturity to produce fully functional chips across a substantial wafer area, enabling chip-level evaluation of threshold voltage (Vth) distribution and retention. This technology achieves an 11% reduction in read time (tR), a 6.9% narrower Vth distribution width, and a 45% improvement in high-temperature retention after cycling compared to conventional continuous CTN cells. These results suggest the current tier pitch limit could be reduced by 4 nm in terms of Vth distribution and by more than 10 nm from a retention perspective, supporting our CTI technology as a compelling solution for continued 3D NAND scaling.

关键技术指标

指标数值说明
读取时间 tR降低 11%与常规连续CTN单元相比的芯片级读取时间改善
Vth分布宽度收窄 6.9%TLC编程后多晶圆全功能芯片的阈值电压分布宽度对比
高温循环后保持特性提升 45%循环后高温数据保持能力的改善幅度
单元间(CtC)干扰降低 30%CTI结构相对连续CTN单元的干扰抑制效果
高k CTN的P/E窗口提升 >1 V在缩小层间距的低堆叠测试载体上采用高k电荷陷阱层所得
层间距可缩小量4 nm(Vth分布)/ >10 nm(保持特性)基于上述结果推算的层间距极限进一步缩小潜力

性能概述

读取时间缩短11%;循环后高温保持特性提升45%(Vth分布宽度收窄6.9%)

技术路线

电荷俘获、垂直堆叠、原子层沉积(ALD)、变异分析、热稳定性

应用场景

高密度3D NAND闪存、数据中心固态存储、高比特密度存储