本文报道了一种为nMOS与pMOS集成不同沟道的单片CFET(mCFET)。我们在常规mCFET工艺基础上,引入了(110)Si pMOS与(100)Si nMOS的晶向组合,以及通过层转移实现的单层嵌入式中间介质隔离(eMDI)。采用该先进衬底,这两项新特征可以以最小的改动集成到任何mCFET基线流程中,且相比替换式MDI(rMDI)集成降低了工艺复杂度。文中报道了采用SiCN eMDI的功能性PMOS与NMOS器件,并评估了与键合介质界面以及SiCN MDI中碳含量相关的关键问题。
This work reports on the demonstration of a monolithic-CFET (mCFET) integrating different channels for nMOS and pMOS. We enhanced our conventional mCFET process with a (110) Si pMOS - (100) Si nMOS combination and a single film embedded middle dielectric insulator (eMDI) by means of layer transfer. Using this advanced substrate, these two new features can be integrated in any mCFET baseline with minimal modifications and reduced process complexity compared to a replacement MDI (rMDI) integration. Functional PMOS and NMOS devices featuring SiCN eMDI are reported. Key aspects related to the bonding dielectric interface and the C content in SiCN MDI are assessed.
| 指标 | 数值 | 说明 |
|---|---|---|
| 嵌入式MDI厚度 | 15 nm | PECVD SiCN单层嵌入式中间介质隔离最薄可做到15nm,体现该集成方案面向未来CFET节点的可缩放性 |
| 键合界面氧化层厚度/氧浓度 | 约6 nm / 约60% O | 亲水键合产生的氧化界面,可在后续清洗中造成横向侵蚀 |
| 界面氧浓度优化 | 20% | 改用远程氢气等离子体活化可使界面氧降至20%,但键合强度明显下降 |
| 堆叠沟道数 | 1-on-1 与 2-on-2 | 已 fabricated 的堆叠Si沟道构型 |
| SiGe牺牲层Ge含量 | 25%(Si0.75Ge0.25) | eMDI方案可提高SiGe中Ge含量,从而改善对内沟道隔离形成与纳米片释放的刻蚀选择比 |
| 键合介质沉积温度 | 500°C(PEALD oxide)/ 350°C(PECVD SiCN) | 分别对应20%与30%碳含量的SiCN MDI成膜条件 |
嵌入式SiCN MDI厚度薄至15nm;键合界面氧化层约6nm(氧浓度约60%)
CFET、垂直堆叠、转移与剥离、单片3D集成、晶圆键合
先进逻辑、高性能计算