我们研究了双栅(DG)氧化铟锡(ITO)FET在室温(RT)、85 °C和125 °C下的正偏压温度不稳定性(PBTI)。我们报道了创纪录低的阈值电压漂移:在125 °C下顶栅应力(2 V)时∆Vth约-37.8 mV。在相同应力条件下,温度较高时ΔVth减小,且Vth恢复比室温更慢。仿真表明高温会退火浅能级陷阱并激活深能级陷阱,但这些效应是暂时的。这些观察结果对ITO晶体管采用高温加速可靠性测试的有效性提出了质疑,因为该测试可能无法反映AOS器件的长期不稳定性。
We study positive bias temperature instability (PBTI) in a dual-gated (DG) indium tin oxide (ITO) FET at room temperature (RT), 85 °C and 125 °C. We report record low threshold voltage shift, ∆Vth ~ -37.8 mV for top gate stress (2 V) at 125 °C. At higher temperatures, ΔVth is reduced and Vth recovery is slower than at RT under identical stress. Simulations show elevated temperatures anneal shallow traps and activate deep-level traps, but these effects are temporary. These observations question the validity of elevated temperature accelerated reliability testing for ITO transistors, as it may not reflect long-term AOS device instability.
| 指标 | 数值 | 说明 |
|---|---|---|
| 阈值电压漂移 ΔVth | -37.8 mV | 125 °C、顶栅+2 V应力(高于常规工作场强)下测得的创纪录低漂移,为AOS器件中最低报道值 |
| 阈值电压漂移 ΔVth | -28 mV | 85 °C、顶栅+2 V应力下的ΔVth,同样低于室温结果 |
| 恢复时间指数 n | -0.03(125 °C)vs -0.4(RT) | 顶栅应力后电流恢复的幂律指数,高温下显著减小,表明恢复更慢 |
| 沟道长度 Lch | 700 nm | 所测试器件的代表性沟道长度(统计25个器件) |
| 测量延迟 | 100 ns | 超快MSM(UF-MSM)方案中应力撤除到测量的延迟,用于捕捉即时恢复 |
| 栅介质厚度 | 8 nm HfO2 | 顶栅与底栅介质均为200 °C PEALD 沉积的HfO2,ITO沟道厚4 nm |
顶栅2 V应力下ΔVth仅-37.8 mV(125 °C),为AOS器件报道最低值;ΔVth -28 mV @85 °C
BTI、电荷俘获、热稳定性
先进逻辑BEOL晶体管、单片3D集成、高可靠AOS器件评估