WaytoICT › 香农学术库 › IEDM 2025 › 论文

GaN快速雪崩器件的首次演示

First Demonstration of GaN Fast Avalanche Device
功率与宽禁带器件短路与雪崩鲁棒性光电二极管III-V3D/2.5D封装实验+仿真
IEDM 2025西安电子科技大学
首次实验实现GaN垂直PIN雪崩脉冲器件,功率密度1.68 GW/cm²、上升时间93 ps、峰值电压2.57 kV。

基本信息

作者
Zhiqing Yang1#, Ming Xiao1#*, Zihan Lin1, Yu Wen1, Kui Dang1, Xiufeng Song1, Shenglei Zhao1, Kai Su1, Zeyang Ren1, Yajie Wang2, Xiaopeng Jing2, Jinfeng Zhang1*, Yue Hao1, Jincheng Zhang1*
机构
西安电子科技大学
国家
中国
会议
IEDM 2025(International Electron Devices Meeting)
电路架构
集成GaN APD-储能电容(Ce)共封装三端模块(In/Out/GND),脉冲测试电路采用50 Ω阻性负载

摘要

我们报道了首个基于GaN的高性能、高压快速雪崩脉冲器件(APD)的实验演示。本工作在原生GaN衬底上制备了快速APD,采用了斜场板与小角度结终端扩展结构。器件展现出高达1.68 GW/cm²的超高峰值输出功率密度、最短93 ps的上升时间、2.57 kV的峰值输出电压以及2.41 kV的陡化电压范围。所实现的功率密度超过Si和GaAs APD两个数量级以上,比SiC同类器件高数十倍。为解决热挑战并提升重复工作性能,我们开发了集成GaN APD模块,采用金刚石热沉与GaN衬底减薄工艺。共封装的储能电容与APD结构使半径为500 μm和50 μm的器件分别获得0.73 K/W和26.1 K/W的低热阻,前者仅为采用AlN和Cu热沉时数值的18%和12%。这些结果证明了GaN宽禁带半导体在下一代高速、高功率雪崩脉冲应用中的巨大潜力。

Abstract

We report the first experimental demonstration of a high-performance, high-voltage fast avalanche pulse device (APD) based on GaN. In this work, we fabricate fast APDs on native GaN substrates, incorporating slanted field plates and small-angle junction termination extensions. The device exhibits an ultra-high peak output power density of 1.68 GW/cm², a minimum rise time of 93 ps, a peak output voltage of 2.57 kV, and a steepened voltage range of 2.41 kV. The achieved power density surpasses that of Si and GaAs APDs by over two orders of magnitude and is tens of times higher than that of SiC counterparts. To address thermal challenges and enhance repetition performance, we developed an integrated GaN APD module featuring a diamond heat sink and GaN substrate thinning. The co-packaged energy storage capacitor and APD structure yields low thermal resistances of 0.73 and 26.1 K/W for devices with radii of 500 and 50 μm, respectively, with the former reaching just 18% and 12% of the values obtained using AlN and Cu heat sinks. These results demonstrate the strong promise of GaN wide-bandgap semiconductors for next-generation high-speed, high-power avalanche pulse applications.

关键技术指标

指标数值说明
峰值输出功率密度1.68 GW/cm²较Si APD高100倍以上,较SiC高数十倍
最小上升时间93 ps50 μm半径器件的输出脉冲上升沿
峰值输出电压2570 V输出脉冲峰值电压,对应陡化电压范围2410 V
雪崩电压1740 V @ 1 mA起始雪崩1650 V,器件可耐1 mA@1740 V不失效
模块热阻0.73 K/W(500 μm)与26.1 K/W(50 μm)金刚石热沉共封装结构,仅为AlN/Cu热沉的18%和12%
导通特性开启电压3.2 V,开关比>10¹²50 μm半径器件正向特性,表明欧姆接触与PN结质量良好

性能概述

峰值输出功率密度 1.68 GW/cm²;最小上升时间 93 ps;峰值输出电压 2.57 kV

技术路线

外延生长、图案化与光刻、选择性刻蚀、热界面材料、热稳定性

应用场景

脉冲功率系统、材料科学与生物医学、电磁发射与核超快过程模拟

打开交互版 · AI 解读 / 同类对比 / 完整指标在香农学术库中查看(需会员)

同领域论文

← 返回香农学术库
蜀ICP备2020035321号-2