WaytoICT › 香农学术库 › IEDM 2025 › 论文

面向亚10nm单元-外围(COP)垂直沟道DRAM晶体管的热稳定高可靠非晶氧化物半导体晶体管

Thermally Robust, Highly Reliable Amorphous Oxide Semiconductor Transistors for sub-10nm Cell-On-Peri Vertical Channel DRAM Transistors
存储器技术DRAMDRAM单元薄膜晶体管(TFT)氧化物半导体(IGZO/ITO)单片集成实验+仿真
IEDM 2025Samsung Advanced Institute of Technology
首次实现耐550℃非晶InGaO垂直沟道晶体管,Vt漂移<0.1 eV、BTI仅-8 mV,可用于单片COP DRAM。

基本信息

作者
Kyooho Jung,#, Ha-Jun Sung#, Yunjin Jang#, Kwang-Hee Lee, Daehyuk Son, Youngkwan Cha, Jung-kyun Kim, Na-Rae Han, Hyerim Hong, Moonil Jung, Jee-Eun Yang*, and Sangwook Kim*
机构
Samsung Advanced Institute of Technology
国家
韩国
会议
IEDM 2025(International Electron Devices Meeting)
工艺节点
sub-10nm(标题所述目标单元节点);实验VCT沟道长度100 nm
供电电压
未提及(BTI应力场为–2 MV/cm)
工作温度
退火550 ℃;BTI测试85 ℃
电路架构
未提及(面向COP单片集成的垂直沟道DRAM单元晶体管)

摘要

我们首次展示了热稳定的非晶InGaO(a-IGO)垂直沟道晶体管(VCT),其沟道长度为100 nm,可耐受高达550 ℃的高温,从而使其能够集成到单片单元-外围(COP)DRAM架构中。氧化物半导体沟道的热退化长期以来是实现DRAM兼容晶体管的主要瓶颈,因为这些晶体管必须承受至少550 ℃的中段制程(MEOL)工艺温度,而传统铟基氧化物在350 ℃以上就会退化。在此,我们提出了在550 ℃贫氧条件下暴露后仍能保持电学性能的非晶氧化物半导体晶体管,所用材料与MEOL/BEOL工艺集成友好。经550 ℃ N₂退火后,器件的阈值电压漂移低于0.1 eV,漏极电流退化可忽略。优异的偏置温度不稳定性(BTI)可靠性(在–2 MV/cm、85 ℃、2000 s条件下ΔVt = –8 mV)可支撑超过10年的稳健工作。分子动力学(MD)与密度泛函理论(DFT)仿真揭示,其热稳定性源于沟道-电极界面处阳离子与阴离子外扩散被抑制。

Abstract

We demonstrate, for the first time, thermally stable amorphous InGaO (a-IGO) vertical channel transistors (VCTs) with a 100 nm channel length that endure up to 550 °C, enabling their integration into monolithic cell-on-periphery (COP) DRAM architectures. Thermal degradation of oxide semiconductor channels has long been a major bottleneck in realizing DRAM-compatible transistors, as they must withstand mid-end-of-line (MEOL) process temperatures of at least 550 °C, while conventional indium-based oxides degrade above 350 °C. Here, we present amorphous oxide semiconductor transistors that retain electrical performance after exposure to 550 °C oxygen-deficient conditions, utilizing integration-friendly materials for MEOL/BEOL processes. After 550 °C N₂ annealing, the devices exhibit a threshold voltage shift below 0.1 eV and negligible drain current degradation. Excellent bias temperature instability (BTI) reliability (ΔVt = –8 mV at –2 MV/cm, 85 °C, 2000 s) supports robust operation beyond 10 years. Molecular dynamics (MD) and density functional theory (DFT) simulations reveal that thermal stability stems from suppressed cation and anion outdiffusion at the channel–electrode interface.

关键技术指标

指标数值说明
热耐受温度550 ℃经550 ℃ N₂退火(贫氧条件)后器件仍保持电学性能
阈值电压漂移< 0.1 eV550 ℃退火后Vt漂移小于0.1 eV,漏极电流退化可忽略
BTI ΔVt–8 mV在–2 MV/cm、85 ℃、2000 s应力条件下,支撑10年以上工作寿命
沟道长度100 nm所演示a-IGO垂直沟道晶体管的沟道长度
退火后Vt0 Va-IGO VCT在550 ℃退火后阈值电压保持在0 V附近

性能概述

550 ℃退火后阈值电压漂移 < 0.1 eV;BTI ΔVt = –8 mV(–2 MV/cm、85 ℃、2000 s)

技术路线

VFET、热稳定性、BTI、退火优化、单片3D集成

应用场景

DRAM、单片三维集成(cell-on-periphery)、高密度先进存储

打开交互版 · AI 解读 / 同类对比 / 完整指标在香农学术库中查看(需会员)