本文通过系统的实验与建模研究,回应了作者此前提出的用于无pass disturb垂直NAND存储的双端口铁电FET(FeFET)架构所面临的挑战。该架构在存储串芯部引入与串工艺兼容的独立pass栅(钝化栅),专门用于pass操作,而不再依赖同一个写栅。主要发现如下:i)非铁电pass栅凭借其几何结构确保了对pass disturb的免疫——pass电压有助于高阈值电压(HVT)态的保持,而其对低阈值电压(LVT)态的不利影响被沟道有效屏蔽;ii)一个关键挑战是HVT态漏电流增大,原因是前栅无法完全耗尽弱的背沟道区域,这一点已通过TCAD建模与实验演示得到验证;iii)为缓解该问题,我们借助TCAD仿真探索了pass栅氧化物与沟道厚度的设计空间,并利用双端口栅侧注入(GSI)FeFET进行了实验验证;iv)所给出的示例设计在实施后展现出无pass disturb工作,同时有效兼顾了漏电折衷;v)另一个挑战是当未选中单元保持HVT态时LVT态的ON电流下降,可通过施加适当的pass栅偏压加以缓解。
In this work, we present comprehensive experimental and modeling studies addressing the challenges of our previously proposed dual-port ferroelectric FET (FeFET) architecture for pass disturb-free vertical NAND storage. This architecture incorporates a string-compatible independent pass gate within the string core, which is dedicated for pass operation rather than relying on the same write gate. Our key findings are as follows: i) The non-ferroelectric pass gate ensures pass disturb immunity via its geometry—pass voltage aids retention of the high-threshold voltage (HVT) state, while the its adverse influence on the low-threshold voltage (LVT) state is effectively screened by the channel; ii) A critical challenge is the increased leakage current in the HVT state, attributed to a weak back-channel region not fully depleted by the front gate, which is verified via both TCAD modeling and experimental demonstration; iii) To mitigate this, we explore the design space of the pass gate oxide and channel thickness through TCAD simulations, and experimentally validate the modeling using dual-port gate-side injection (GSI) FeFETs; iv) The example design, when implemented, demonstrates pass disturb-free operation while effectively managing the leakage trade-off; v) Another challenge is reduced ON-current for LVT state when unselected cells remain in HVT states. This can be mitigated by applying proper pass gate biases.
| 指标 | 数值 | 说明 |
|---|---|---|
| 沟道厚度 | 25 nm | 多晶硅沟道,沉积于背栅介质之上 |
| 背栅介质厚度 | 25 nm | SiO2背栅介质,独立pass栅所用电介质 |
| 铁电层厚度 | 10 nm | Hf0.5Zr0.5O2(HZO)铁电层,位于控制栅叠层 |
| 电荷俘获层厚度 | 3.5 nm | SiNx电荷俘获层,构成混合栅叠层 |
| HVT态漏电流趋势 | 随背栅VPASS指数上升 | TCAD与双端口GSI FeFET实验共同验证 |
背栅VPASS下HVT态漏电流呈指数上升;示例设计采用25 nm多晶硅沟道与25 nm SiO2背栅介质实现pass disturb-free工作
铁电极化、垂直堆叠
3D NAND存储、高密度非易失存储、低功耗写入NAND