WaytoICT › 香农学术库 › IEDM 2025 › 论文

用于Core与I/O RMG栅叠层的新型低温氧氢自由基SiO2形成工艺:以无电荷界面层实现极致NBTI可靠性

Novel Low Temperature SiO2 Formation Process by Oxygen and Hydrogen Radicals for Core and I/O RMG Stacks: Achieving the Ultimate NBTI Reliability with a Charge-Free IL
建模与可靠性BTI与热载流子MOSFET/FinFET硅基CMOS实验
IEDM 2025imec
用氧氢自由基等离子体在450°C形成无固定电荷SiO2界面层,NBTI可靠性超越900°C干氧工艺。

基本信息

作者
J. Franco*, H. Arimura, J. P. Bastos, V. Afanas'ev1, J.-F. de Marneffe, M.-S. Kim, B. Kaczer, N. Horiguchi
机构
imec
国家
比利时
会议
IEDM 2025(International Electron Devices Meeting)
供电电压
Core Logic 过驱动电压 Vov 最高1.34 V,I/O 最高1.98 V(对应1.8V I/O技术)
工作温度
未提及(工艺温度450°C,对比900°C干氧)
电路架构
未提及(采用MOS电容器测试结构,HKMG为1.9nm HfO2/5nm TiN)

摘要

未来CMOS架构需要低热预算的RMG集成。我们展示了一种新型低温(450°C)等离子体基SiO2形成工艺,利用氧和氢自由基获得低缺陷、无固定电荷的界面层,其性能优于常规SiO2形成工艺,包括900°C干氧氧化。界面层厚度可在对Core Logic与I/O栅叠层有意义的范围内进行控制(本文演示0.75-2nm),而仅靠常规自限制化学氧化无法做到。该新型界面层由于抑制了空穴俘获并使界面态产生最小化,无需任何生长后处理即可实现极致NBTI可靠性。通过与经各种处理的常规chemOx界面层的对比分析,揭示了SiO2正固定电荷(被俘获的质子)在NBTI应力期间对空穴俘获与界面态去钝化的作用。

Abstract

Low thermal budget RMG integration is required for future CMOS architectures. We demonstrate a novel low-temperature (450°C) plasma-based SiO2 formation process by oxygen and hydrogen radicals yielding a low-defectivity, fixed charge-free interfacial layer, and outmatching conventional SiO2 formation processes, including a 900°C dry oxidation. IL thickness control is demonstrated in the range of relevance for Core Logic and I/O gate stacks, which would not be possible with conventional self-limited chemical oxidation only. The novel IL enables ultimate NBTI reliability due to suppressed hole trapping and minimized interface state generation, without requiring any post-growth treatment. A comparative analysis vs. conventional chemOx IL with various treatments sheds light on the role of SiO2 positive fixed charge (trapped protons) on hole trapping and interface state de-passivation during NBTI stress.

关键技术指标

指标数值说明
固定正电荷密度 Qfix+< 2×10^11 /cm2比900°C干氧热氧化层低约2.5倍,体电荷密度可忽略
工作氧化场 Eox~8 MV/cm在IL厚度0.75-2nm范围内均保持,且无NBTI可靠性劣化
界面层厚度控制范围0.75-2 nmO*H*工艺可调,突破常规chemOx自限制约1nm的限制
泄漏电流同物理厚度下降低约10倍相对常规界面层的漏电改善
介电常数 k3.9接近化学计量比SiO2的名义值,而chemOx IL约为6.9(缺陷导致)
工艺温度450°C远低于900°C干氧与850°C spike退火

性能概述

固定正电荷密度 Qfix+ < 2×10^11 /cm2(比900°C干氧低约2.5倍);工作氧化场 Eox ~8 MV/cm

技术路线

高k金属栅、低温工艺、BTI、电荷俘获

应用场景

先进逻辑(Core Logic)、I/O器件、CFET与顺序3D集成

打开交互版 · AI 解读 / 同类对比 / 完整指标在香农学术库中查看(需会员)

同领域论文

← 返回香农学术库
蜀ICP备2020035321号-2