WaytoICT › 香农学术库 › IEDM 2025 › 论文

通过氢退火改善IGZO晶体管PBTI可靠性,在95°C下实现5年寿命的1.2V过驱动电压

Improving IGZO transistor PBTI reliability with hydrogen anneal achieving overdrive voltage of 1.2V for a lifetime of 5 years at 95°C
新型沟道与材料器件氧化物半导体FET薄膜晶体管(TFT)氧化物半导体(IGZO/ITO)实验+仿真
IEDM 2025imec
提出氢退火加氧退火方案,抑制IGZO晶体管PBTI中的氢掺杂退化约30倍,实现95°C下5年寿命的1.2V过驱动电压。

基本信息

作者
A. Chasin*, J. Franco, D. Matsubayashi, S. Tyaginov, M.J. van Setten, B. De Wachter, H. Dekkers, A. Kruv, P. Rinaudo1, Y. Zhao, L. Panarella1, V. Afanas'ev1, A. Pavel, Y. Wan, S. Subhechha, A. Belmonte, B. Kaczer, G. S. Kar
机构
imec
国家
比利时
会议
IEDM 2025(International Electron Devices Meeting)
供电电压
过驱动电压 Vov = VG,stress − Vth0,寿命目标对应 Vov,max = 1.2 V;可靠性判据在 Vov = 1.5 V 下考核
工作温度
25°C 与 125°C 表征测试;目标工作条件 95°C
电路架构
面向 1T1C 与 2T0C DRAM 集成方案(仅提及,未实现阵列)

摘要

我们提出一种用于IGZO基晶体管的新型退火方案,可获得满足嵌入式DRAM应用可靠性指标所需的抗氢能力:在95°C下、5年寿命内实现1.2V的过驱动电压。首先,我们表明标准IGZO组分(约1:1:1 at%)与贫铟(In约10%)组分存在相反的可靠性限制。标准IGZO仅能满足由电子俘获引起的+ΔVth分量的可靠性目标,贫铟组分则仅能满足由氢掺杂引起的-ΔVth分量的可靠性目标。我们将贫铟薄膜中观察到的约10倍更大的+ΔVth归因于IGZO导带Ec与Al2O3陷阱带之间更接近的能量对齐。其次,我们描述氢退火(FGA)与氧退火的组合如何在不造成性能损失的情况下,将PBTI应力过程中的氢掺杂过程降低约30倍。该可靠性提升被认为源于FGA过程中对过量氧的清除作用,从而最大限度地减少了高温PBTI期间由栅介质释放的氢的优先成键位置。

Abstract

We propose a novel annealing scheme for IGZO-based transistors, which enables the hydrogen resilience needed to meet the reliability specs for embedded DRAM applications: an overdrive voltage of 1.2V for a lifetime of 5 years at 95°C. First, we show that standard IGZO compositions (~1:1:1 at%) and In-poor (In~10%) suffer from opposite reliability limitations. Standard IGZO only meets the reliability target for the +ΔVth component caused by electron trapping, In-poor only meets the reliability target for the -ΔVth component caused by H-doping. We ascribe the observed ~10x larger +ΔVth in In-poor films to a closer energetic alignment between IGZO Ec and Al2O3 trap bands. Second, we describe how a combination of hydrogen (FGA) and oxygen anneals reduces the H-doping process during PBTI stress by ~30x, without a performance penalty. This reliability improvement is reasoned to be due to excess oxygen scavenging during FGA, minimizing the preferential bonding sites of hydrogen released by the gate-dielectric during PBTI at high temperatures.

关键技术指标

指标数值说明
最大过驱动电压 Vov,max1.2 V在95°C、5年连续直流工作寿命下满足|ΔVth|≤70 mV的过驱动电压
可靠性判据 |ΔVth|70 mVVov = 1.5 V、EOT = 2.5 nm、95°C下工作5年的工业相关判据
H掺杂退化改善约30倍氢退火(FGA)与氧退火组合使PBTI应力中的H掺杂过程降低约30倍且无性能损失
贫铟薄膜+ΔVth差异约10倍In-poor薄膜相比标准IGZO的+ΔVth大约10倍,源于能带对齐更接近Al2O3陷阱带
退化激活能 EA约50 meV / 约500 meV分别为电子俘获与H掺杂过程的激活能,用于25°C/125°C分离表征
时间幂律因子 n0.16 / 0.25分别为电子俘获与H掺杂过程的时间动力学指数

性能概述

过驱动电压 Vov,max = 1.2 V(95°C、5年寿命);PBTI应力中H掺杂退化降低约30倍

技术路线

退火优化、BTI、电荷俘获

应用场景

嵌入式DRAM(eDRAM)、1T1C/2T0C DRAM集成、先进逻辑后端单片集成