传统电流驱动自旋力矩器件存在能耗高的问题,尽管电压控制的磁电(ME)方案可实现超低能耗工作,但其CMOS集成仍受限于特殊单晶衬底(ABO₃)和约700 ℃的高工艺温度。本文提出一种与CMOS兼容的磁电器件,采用Hf0.5Zr0.5O2(HZO)/Pt纳米团簇异质结构,在硅片上以400 ℃完成制备。Pt纳米团簇通过降低横向Pt/Co界面处Co-O键的解离能垒来增强磁电耦合。该机制提升了HZO铁电极化翻转过程中的氧迁移能力,从而实现电压控制的磁化翻转,能耗极低(0.46 pJ/μm²),显著低于自旋力矩器件(100-1000 pJ/μm²)。该工作为CMOS兼容的低功耗磁电逻辑与存储集成开辟了关键路径。
Conventional current-driven spin torque devices suffer from high energy consumption, though voltage-controlled magnetoelectric (ME) alternatives enable ultra-low-energy operation, their CMOS integration remains constrained by special single-crystal substrates (ABO₃) and high processing temperatures (~700 °C). Here, we developed a CMOS-compatible ME device with Hf0.5Zr0.5O2 (HZO)/Pt-nanocluster heterostructure, which is fabricated at 400°C on silicon wafer. The Pt-nanocluster enhances the ME coupling by reducing the dissociation energy barrier of Co-O bonds at lateral Pt/Co interfaces. This mechanism enhances oxygen mobility during ferroelectric polarization switching in HZO, enabling voltage-controlled magnetization reversal with ultra-low energy consumption (0.46 pJ/μm²) – significantly below spin torque devices (100-1000 pJ/μm²). This establishes a critical pathway for CMOS-compatible, low-power magnetoelectric logic and memory integration.
| 指标 | 数值 | 说明 |
|---|---|---|
| 写入能耗 | 0.46 pJ/μm² | 由单次翻转PUND校正I-V曲线测得,对100 nm器件折算约4.6 fJ/次写入 |
| 归一化剩磁变化 ΔMr/Ms | ≈0.9 | Pt纳米团簇厚度为0.4 nm时取得峰值,远高于无Pt时的<0.2 |
| HZO剩余极化 Pr | 24 μC/cm² | PUND校正的P-V测试证实稳健铁电性,且Pr与Co的Mr/Ms相关联 |
| 翻转速度 | 1 ns @ 3 V(6 μm器件) | 计算表明HZO电容可在3 V下实现约1 ns的磁化翻转速度 |
| 工艺热预算 | 400 ℃ | 在硅片上完成HZO/Pt纳米团簇磁电堆叠制备,与CMOS后端工艺兼容 |
写能耗 0.46 pJ/μm²;归一化剩磁变化 ΔMr/Ms ≈ 0.9
低温工艺、铁电极化、磁翻转
超低功耗存储、磁电逻辑、CMOS后端(BEOL)集成