我们展示了双自旋力矩磁隧道结(DS-MTJ)相比标准单MTJ实现了25%的效率提升,且不劣化其他性能。优化的叠层使4-kbit DS-MTJ阵列的两个参考层能够可靠地设置到所需的反平行(AP)排列,并首次演示了全部4k器件在2 ns写入脉冲下的翻转。借助新的自由层设计,在临界尺寸(CD)约40 nm时实现了约60 kT的激活能,克服了单一氧化物界面DS-MTJ的关键挑战之一。具有优化DS-MTJ自由层的器件还表现出陡峭的写错误率(WER)斜率,与迄今报道的最佳单MTJ相当。
We demonstrate 25% efficiency improvement in double spin-torque magnetic tunnel junctions (DS-MTJs) compared to standard single-MTJs, without degrading other properties. Optimized stacks enabled reliable setting of the two reference layers into the desired anti-parallel alignment for a 4-kbit DS-MTJ array, where switching of all 4k devices with 2 ns write pulses was demonstrated for the first time. Activation energy ~ 60 kT at CD ~ 40 nm was achieved with new free layer designs, overcoming one of the key challenges of DS-MTJs with a single oxide interface. Devices with optimized DS-MTJ free layers also exhibit steep write-error-rate (WER) slopes, comparable to those of the best single-MTJs reported to date.
| 指标 | 数值 | 说明 |
|---|---|---|
| 自旋力矩效率提升 | 25%(最高36%,中位26%) | DS-MTJ相对仅底部参考层单MTJ的效率提升,10 ns写入脉冲、RA约10 Ω·µm² |
| 开关电压/电流降低 | Vc (Ic) 降低 20% | 相对对照单MTJ,在3–10 ns脉宽、39–66 nm尺寸范围内一致,1e-6 WER下同样成立 |
| 激活能 | ~60 kT @ CD ~40 nm | 新型自由层设计在单一氧化物界面下实现,解决DS-MTJ热稳定性不足问题 |
| 最窄写入脉冲 | 2 ns | 4-kbit阵列全部4k器件首次实现2 ns写入脉冲翻转 |
| 隧穿结电阻面积积 | 10 Ω·µm² | 工艺上更具相关性的RA(现有MgO工艺限制使更低RA难实现) |
| 参考层设置偏置场 | 中位 H0 = -320 Oe(标准差73 Oe) | 通过增厚非磁间隔层可将偏置场降至<200 Oe,实现单场可靠设置AP参考层 |
效率提升25%(最高36%);开关电压Vc降低20%(RA=10 Ω·µm²)
磁翻转、热稳定性、变异分析
末级缓存(LLC)、高性能计算与AI加速器、嵌入式非易失存储
打开交互版 · AI 解读 / 同类对比 / 完整指标在香农学术库中查看(需会员)