我们成功演示了世界上首个后段制程(BEOL)集成的多层水平单元堆叠DRAM架构——采用双沟道铟镓锌氧化物(IGZO)FET,并在12英寸晶圆平台上通过实验验证了其可行性。所制备的IGZO基双沟道存取晶体管在Vds=1.0 V、Vgs=2.0 V下实现60.9 µA/μm的开态电流,具有正阈值电压(Vt=0.28 V)、80 mV/dec的亚阈值摆幅,以及低于1 fA/μm的关态电流(受测试极限限制)。此外,器件表现出优异的可靠性,动态PBTI测试表明最大栅压(Vgmax)为1.66 V时可保证100°C下10年寿命,且ΔVt<100 mV。推算的TDDB 10年寿命(100℃)最大栅压为3.62 V。这些性能提升归因于优化策略,包括合适的IGZO组分、界面工程、栅绝缘层(GI)与栅电极薄膜叠层设计,以及降低源漏接触电阻。这一创新架构的突破解决了传统微缩的限制,同时保持关键电学与可靠性阈值,为未来DRAM创新提供了有前景的路径。
We have successfully demonstrated the world's first backend-of-line (BEOL)-integrated, multi-tiered horizontal cell stacked DRAM architecture—featuring a double-channel indium gallium zinc oxide (IGZO) FET—proving its feasibility through experimental validation on a 12-inch wafer platform. The fabricated IGZO-based double-channel access transistor achieved an on-current (Ion) of 60.9 µA/μm at Vds=1.0V and Vgs=2.0V, a positive threshold voltage (Vt=0.28V) with a subthreshold swing of 80 mV/dec, and an off-current (Ioff) below 1fA/μm (test-limited). Additionally, the device demonstrated excellent reliability, a dynamic PBTI testing indicated a maximum gate voltage (Vgmax) of 1.66V ensuring a 10-year lifetime at 100°C with ∆Vt <100 mV. The projected TDDB maximum gate voltage is 3.62 V for 10-years lifetime at 100℃. These performance gains are attributed to optimized strategies, including proper IGZO composition, interface engineering, gate insulator (GI) and gate electrode film stack design, and reduced source/drain contact resistance. The breakthrough in this innovative architecture with addresses conventional scaling limitations while maintaining key electrical and reliability thresholds, offering a promising path for future DRAM innovation.
| 指标 | 数值 | 说明 |
|---|---|---|
| 开态电流 Ion | 60.9 µA/μm | 在Vds=1.0 V、Vgs=2.0 V下测得,源自源漏接触电阻优化后的双沟道IGZO FET |
| 阈值电压 Vt | 0.28 V | 常关型正阈值,配合80 mV/dec的亚阈值摆幅 |
| 关态电流 Ioff | < 1 fA/μm | 受测试设备极限限制,体现IGZO超低泄漏特性 |
| 亚阈值摆幅 SS | 80 mV/dec | 反映栅控能力与界面质量 |
| PBTI 寿命栅压 Vgmax | 1.66 V | 100°C下保证10年寿命且ΔVt<100 mV的最大栅压 |
| TDDB 寿命栅压 | 3.62 V | 推算的100℃下10年寿命最大栅压 |
Ion = 60.9 µA/μm(Vds=1.0 V,Vgs=2.0 V);Ioff < 1 fA/μm(受测试极限限制)
垂直堆叠、单片3D集成、原子层沉积(ALD)、高k金属栅、低温工艺
高密度DRAM存储、云计算与数据中心内存、AI加速器主存
打开交互版 · AI 解读 / 同类对比 / 完整指标在香农学术库中查看(需会员)