WaytoICT › 香农学术库 › IEDM 2025 › 论文

具有独立读写路径的3D可堆叠双栅纳米片(DGNS)FeFET:亚2%误码率下抑制变异性并缓解亚阈值摆幅退化

3D-Stackable Double-Gate Nanosheet (DGNS) FeFETs with Separate Read/Write Paths: Suppressed Variability with Sub-2 % Bit Error Rate and Mitigated Subthreshold Swing Degradation
新兴存储器FeRAM与FeFETFeFETGAA纳米片硅基CMOS铁电HZO实验
IEDM 2025阳明交通大学
首次实验实现双栅纳米片FeFET读写分离,误码率由25.7%降至1.78%,变异性抑制逾37%。

基本信息

作者
F. Wu1, C.-Y. Chiu2, C.-H. Wu3, Y.-L. Tsai2, S.-H. Chen2, H.-C. Lin1, V. P.-H. Hu3, C.-J. Su1,2,*, P. Su1,**
机构
阳明交通大学
国家
中国台湾
会议
IEDM 2025(International Electron Devices Meeting)
供电电压
写电压 Vw = 3.5 V(饱和翻转),可缩放至 2.25 V

摘要

我们首次实验验证了一种双栅纳米片(DGNS)FeFET架构,通过读写路径分离来抑制变异性并提升可靠性。将顶栅(TG)用于编程、侧栅(SG)用于感测,该架构可最小化读干扰、缓解耐久性退化过程中的亚阈值摆幅(SS)退化,并提升对铁电(FE)相不均匀性的免疫能力。与仅用TG感测相比,该设计将误码率从25.7%降至1.78%,并将循环间(C2C)与器件间(D2D)变异性抑制37%以上。本工作填补了此前基于仿真的DG FeFET变异性研究留下的关键实验空白。DGNS方案还支持3D堆叠与低功耗工作。这些改进表明,实现面向非易失存储与存内逻辑应用的可缩放、高可靠FeFET,关键在于架构解耦与界面控制,而非仅依赖铁电材料本征特性。

Abstract

We present the first experimental validation of a double-gate nanosheet (DGNS) FeFET architecture that suppresses variability and enhances reliability through read/write path separation. By assigning the top-gate (TG) for programming and the side-gate (SG) for sensing, the architecture minimizes read disturbance, mitigates subthreshold swing (SS) degradation under endurance, and improves immunity to ferroelectric (FE) phase non-uniformity. Compared to TG-only sensing, this design reduces the bit error rate from 25.7 % to 1.78 % and suppresses cycle-to-cycle (C2C) and device-to-device (D2D) variability by over 37 %. This work fills a critical experimental gap left by prior simulation-based studies on DG FeFET variability. The DGNS scheme further supports 3D stacking and low-power operation. These improvements demonstrate that architectural decoupling and interface control, rather than merely intrinsic FE properties, are key to achieving scalable and reliable FeFETs for non-volatile memory and logic-in-memory applications.

关键技术指标

指标数值说明
误码率(BER)1.78%(TG-only 为 25.7%)侧栅读取相比仅顶栅读取将误码率降低约14倍
C2C/D2D 变异性抑制 >37%读写路径分离后循环间与器件间波动显著减小
存储窗口(MW)~0.4 V(Vw 降至 2.25 V 仍保持)满足可靠态区分与读余量容限
开态电流 Ion提升 >9.1×双栅同时偏置相对仅顶栅工作,栅控增强
写脉冲宽度1 μs固定脉宽下采用幅度调制实现部分到完全翻转
铁电栅堆叠9 nm 超晶格 HZO + 5 nm Si3N4 侧栅介质原位 NH3 表面处理抑制氧空位形成

性能概述

误码率由25.7%降至1.78%;C2C/D2D变异性抑制超过37%

技术路线

GAA、垂直堆叠、铁电极化、变异分析、存内计算

应用场景

嵌入式非易失存储、存内逻辑计算、高密度3D堆叠存储

打开交互版 · AI 解读 / 同类对比 / 完整指标在香农学术库中查看(需会员)

同领域论文

← 返回香农学术库
蜀ICP备2020035321号-2