氧化物半导体(OS)与硅(如多晶硅和单晶硅)的异质集成在推动显示和3DIC发展方面展现出广阔前景,但不可避免的氢(H)掺杂导致了严重的工艺不兼容问题。针对现有抑制方案难以解决H诱发的微米尺度短沟道效应(SCE)以及OS场效应晶体管(FET)中严重的偏压温度不稳定性问题,本文提出了一种全新的、与异质集成兼容的氢疏散层(HEL),使OS FET实现彻底的抗氢化。在OS沟道长度缩小至60 nm时,H诱发的短沟道效应被有效抑制,正/负偏压温度不稳定性(PBTI/NBTI)和自热不稳定性(SHI)分别降至0.03 V和0.3 V。这为微米与纳米尺度OS-Si异质集成铺平了道路。
The hetero-integration of oxide semiconductors (OSs) and silicon (e.g., poly-Si and crystalline-Si) exhibits promising potential on advancing displays and 3DICs, while the inevitable hydrogen (H) doping results in a critical process incompatibility. In contrast to incumbent mitigation solutions to the H-induced micro-scale short-channel effect (SCE) and severe bias-temperature instabilities in OS field-effect transistors (FETs), a novel hetero-integration-compatible Hydrogen Evacuation Layer (HEL) is proposed to enable the thorough hydrogenation-immunity in OS FETs. The H-induced SCE is suppressed with OS channel length downscaling to 60 nm, and positive/negative bias temperature instabilities (PBTI/NBTI) and self-heating instability (SHI) are reduced to 0.03 V and 0.3 V, respectively. This paves the way for Miro- and Nano-scale OS-Si hetero-integration.
| 指标 | 数值 | 说明 |
|---|---|---|
| H扩散长度限制 | 63 nm | HEL通过热力学捕获将氢扩散长度限制在63 nm,与氧空位迁移尺度匹配 |
| PBTI/NBTI 阈值漂移 | < 0.03 V(<30 mV) | 采用HEL后正/负偏压温度不稳定性的阈值电压漂移 |
| 自热不稳定性 SHI | 0.3 V | HEL使自热引起的阈值漂移降至0.3 V(无HEL时比基线恶化45%) |
| 沟道长度 | 60 nm | H诱发短沟道效应被抑制的最小OS沟道长度 |
| H污染下的PBTI漂移(对照) | > 5.8 V | 无HEL、富氢SiOx钝化层污染时80℃ PBTI的阈值漂移 |
| 表面-OH浓度 | 15.4 at%(对照35.2 at%) | 10 nm深度处HEL保护样品保持近原始羟基含量,而无保护样品升至35.2 at% |
PBTI/NBTI 阈值漂移 0.03 V;自热不稳定性(SHI) 0.3 V
原子层沉积(ALD)、BTI、热稳定性
3DIC异质集成、大面积电子与显示、先进逻辑