WaytoICT › 香农学术库 › IEDM 2025 › 论文

面向300mm晶圆叠层沟道FET的ALD MoS2沟道后置集成新方案

Novel channel-last integration of ALD MoS2 into stacked channel FETs on 300mm wafers
新型沟道与材料器件二维材料FETGAA纳米片CFETMOSFET/FinFET二维材料(TMD)硅基CMOS实验+仿真
IEDM 2025未提及
首次实现ALD MoS2沟道后置集成到300mm叠层沟道FET,Nb接触RcW低至54 kΩ·µm。

基本信息

作者
S. Barraud1, M. Rodriguez-Fano1, J.M. Pedini1, S. Cadot1, R. Chouk1, B. Dey1, J.M. Hartmann1, A. Gharbi1, C. Comboroure1, A. Sarrazin1, F. Boulard1, L. Laraignou1, A. Campo1, H. Grampeix1, C. Castan1, J. Sturm1, A. Souhaité1, A. Lassenberger1, L. Couture1, D. Mariolle1, P. Hauchecorne1, V. Loup1, E.
机构
未提及
国家
法国
会议
IEDM 2025(International Electron Devices Meeting)

摘要

我们首次报道了通过一种新型沟道后置集成方案,将ALD生长的MoS2集成到叠层沟道晶体管中。该方法在沟道形成、改善剥离(分层)控制、接触优化、降低交叉污染风险以及复用现有Si GAA工艺模块等方面带来诸多优势与机会。为评估该工艺流程,我们首先开发并优化了ALD MoS2薄膜,并利用沟道宽度缩小至15 nm的背栅MoS2晶体管优化了源漏接触。铌(Nb)接触实现了高达10⁴的ION/IOFF比,并相较钛(Ti)接触将ION最高提升28倍。随后,我们验证了该新型沟道后置集成的关键工艺模块,克服了限制2D TMD集成到先进CMOS中的大部分技术障碍。最后,我们通过TCAD仿真优化了器件架构并给出了未来展望。

Abstract

We report, for the first time, the integration of ALD-grown MoS2 into stacked channel transistors via a novel channel-last integration scheme. Our approach provides many advantages and opportunities concerning channel formation, enhanced delamination control, contact optimization, reduced contamination risks, and the ability to reuse process modules of existing Si GAA routes. To assess such a process flow, we first developped and optimized ALD MoS2 films. We also optimized source/drain contacts using back-gated MoS2 transistors with down to 15 nm widths. Niobium contacts delivered an ION/IOFF ratio up to 10⁴ and outperformed titanium counterparts with up to 28× Iₒₙ enhancement. Then, we validated key modules of our novel channel-last integration, overcoming most of the technological roadblocks limiting the 2D TMD integration into advanced CMOS. Finally, TCAD simulations were performed to optimize our architecture and draw some perspectives.

关键技术指标

指标数值说明
接触电阻RcW54 kΩ·µm用TLM法提取的最窄沟道(15 nm)器件的接触电阻
开关比ION/IOFF10⁴Nb/NbN环绕接触背栅MoS2 FET达到的最高开关比
ION提升倍数28×Nb接触相比Ti接触的ION提升,源于更低的阈值电压与接触电阻
最小沟道宽度15 nmDUV与电子束光刻结合RIE刻蚀实现的MoS2纳米带宽度
MoS2厚度范围1-10 MLALD沉积的MoS2单层数范围,器件采用3与6 ML

性能概述

接触电阻RcW = 54 kΩ·µm;ION/IOFF最高达10⁴(Nb接触较Ti接触ION提升28倍)

技术路线

原子层沉积(ALD)、垂直堆叠、GAA、CFET

应用场景

先进逻辑、超越Si的CMOS微缩、三维堆叠器件