WaytoICT › 香农学术库 › IEDM 2025 › 论文

面向3D V-NAND闪存可靠PLC工作的能带工程氮氧化硼隧穿层

Bandgap-Engineered Boron Oxynitride Tunneling Layer for Reliable PLC operation of 3D V-NAND Flash Memory Devices
存储器技术3D NAND3D NAND硅基CMOS实验
IEDM 2025Korea Advanced Institute of Science and Technology
以氮氧化硼BON替代SiON作3D V-NAND隧穿层,降低价带偏移加快擦除并抑制陷阱,实现可靠PLC。

基本信息

作者
Dae Hyun Kang1, Jaejoong Jeong1, Youngkeun Park1, Yungjun Kim2, Dong Hun Sin3, Han Mei Choi3 and *Byung Jin Cho1, 2
机构
Korea Advanced Institute of Science and Technology
国家
韩国
会议
IEDM 2025(International Electron Devices Meeting)
工作温度
室温与85℃(保持特性测试)

摘要

我们提出氮氧化硼(BON)作为一种新型隧穿层材料,可替代传统SiO2/SiON/SiO2隧穿层叠层中的SiON。与SiON相比,BON相对于硅具有更小的价带偏移和更大的导带偏移。这些特性增强了擦除过程中的空穴注入,并降低了保持状态下的电子损失。BON的这些特性有助于克服闪存擦除效率与可靠性之间的权衡。与采用SiON隧穿层叠层的器件相比,采用BON隧穿层叠层的存储器件展现出陡峭25.4%的ISPE斜率、循环前快9倍、循环后快23倍的擦除速度。此外,BON显著降低了陷阱产生,从而带来更优的保持特性、耐久性以及更窄的单元间涨落。因此,它成功实现了可靠的五阶单元(PLC)工作,与采用SiON隧穿层的对照器件相比,标准差降低3倍,态间裕度增大4倍。

Abstract

We introduce Boron Oxynitride (BON) as a novel tunneling layer material which can replace SiON in the conventional SiO2/SiON/SiO2 tunneling layer stack. Compared to SiON, BON exhibits a smaller valence band offset and a larger conduction band offset with respect to silicon. These properties enhance hole injection during erase operation and reduce electron loss during retention. These characteristics of BON help overcome the tradeoff between erase efficiency and the reliability of flash memory. A memory device with a BON tunneling layer stack shows 25.4% steeper ISPE slope, 9 times faster erase before cycling, and 23 times faster erase after cycling, compared to a device with a SiON tunneling layer stack. Furthermore, BON significantly reduces trap generation, resulting in superior retention, endurance, and narrower cell-to-cell variation. Consequently, it successfully enables reliable Penta-Level-Cell (PLC) operation, achieving a 3 times lower standard deviation and a 4 times larger state-to-state margin compared to the control device with SiON tunneling layer.

关键技术指标

指标数值说明
ISPE斜率-0.86 V/VBON器件编程-擦除斜率较SiON的-0.69 V/V陡峭25.4%,表明擦除效率更高
擦除速度提升9倍(循环前)/23倍(1k次P/E循环后)以VFB从+4 V移至-4 V所需时间计,循环后优势由9倍扩大到23倍
能带偏移VBO低0.98 eV、CBO高0.48 eVBON相对SiON对硅的价带偏移更小、导带偏移更大,带隙5.83 eV、Evac-EVBM为6.91 eV
保持特性10^4 s后电子损失约减半室温与85℃下编程态电荷损失均约为SiON器件的一半
耐久性10^4次P/E循环BON器件10^4循环内稳定工作,SiON在10^3循环后VFB显著下降
PLC分布标准差低3倍、态间裕度大4倍相对SiON对照器件,支持可靠的五阶单元工作

性能概述

ISPE斜率-0.86 V/V(较SiON的-0.69 V/V改善25.4%);1k次P/E循环后擦除速度快23倍

技术路线

电荷俘获、变异分析

应用场景

3D NAND闪存、高密度存储(QLC/PLC)、数据中心存储

打开交互版 · AI 解读 / 同类对比 / 完整指标在香农学术库中查看(需会员)

同领域论文

← 返回香农学术库
蜀ICP备2020035321号-2