微缩FeFET中局域铁电相变化研究:实验与建模

On the Localized Ferroelectric Phase Variation in Scaled FeFET: Experiments and Modeling
新兴存储器FeRAM与FeFETFeFET硅基CMOS铁电HZO实验+仿真
IEDM 2025Georgia Institute of Technology
实验发现并TCAD建模28nm FeFET中局域铁电/介电相分布致VTH漂移(LPTS),电容读取更抗相变。

基本信息

作者
Omkar Phadke1, Minji Shon1, Stuart Wodzro1, Halid Mulaosmanovic2, Stefan Dünkel2, Sven Beyer2, Asif Khan1, Suman Datta1, Shimeng Yu1
机构
Georgia Institute of Technology
国家
美国
会议
IEDM 2025(International Electron Devices Meeting)
工艺节点
28nm 体硅 FeFET 平台
供电电压
写入 ±5 V;读取 50 mV – 1 V(VDS/VSD)
工作温度
室温(room temperature,保持特性测试)
电路架构
TCAM(SPICE案例研究)、1FeFET-C单元、AND型伪交叉阵列

摘要

铁电薄膜中的相变化是铁电场效应晶体管(FeFET)阈值电压(VTH)波动的主要原因。本工作评估了“局域化”铁电/介电(FE/DE)相变化对FeFET的影响,并通过实验表征了一种新现象,即局域相分布诱导阈值电压漂移(LPTS)。在此,微缩FeFET表现出非对称的电流读取特性,导致阈值电压(VTH)漂移依赖于电流流动方向(当源漏互换时)。器件表征(包含器件间与循环间波动)在28 nm体硅FeFET技术平台上完成。配套TCAD仿真表明,源端-沟道与漏端-沟道边界附近FE/DE相数量不均是造成非对称电流读取的主要原因。此外,仿真表明,相较于传统电流读取,微缩FeFET新型非破坏性“电容”读取对相变化更鲁棒,因为LPTS效应被摊薄/抵消。

Abstract

Phase variations in the ferroelectric thin films are the primary cause of the threshold voltage (VTH) variation in the Ferroelectric Field Effect Transistor (FeFET). In this work, the impact of "localized" ferroelectric/dielectric (FE/DE) phase variation on FeFET is evaluated. A new phenomenon, namely, Localized Phase Distribution Induced Threshold Voltage Shift (LPTS), is experimentally characterized. Here, a scaled FeFET exhibits an asymmetric current readout that leads to a threshold voltage (VTH) shift that is dependent on the direction of current flow (when source and drain are flipped). The device characterization with device-to-device and cycle-to-cycle variations is performed on 28 nm bulk Si FeFET technology platform. The supporting TCAD simulations point towards the presence of an uneven number of FE/DE phases near Source-Channel vs Drain-Channel boundary to be the main cause of asymmetric current readout. Further, the simulation indicates that the novel non-destructive "capacitive" readout of a scaled FeFET to be more robust towards phase variation compared to the traditional current readout as the LPTS effect is amortized.

关键技术指标

指标数值说明
读电压50 mV / 1 V低读电压下IDS与ISD读取对称,1V高读电压下出现VTHD与VTHS不等的非对称读取
写脉冲条件±5 V, 10 µs栅极写入脉冲幅度与宽度,足以完成编程/擦除
铁电剩余极化±10 µC/cm2TCAD中14nm×14nm方形铁电相晶粒所采用的Pr值
保持时间>1000 s室温下ON态保持测试中非对称性维持超过1000秒
耐久循环100 P/E cycles循环间测试显示非对称读取特性在100次编程/擦除循环内保持
器件尺寸W/L = 80nm/80nm 与 1000nm/80nm窄宽度器件ΔVTH分布更分散,宽器件分布更集中

性能概述

高读电压1V下ΔVTH=VTHD-VTHS呈随机不对称(低读电压50mV下对称);铁电相Pr=±10 µC/cm2

技术路线

铁电极化、变异分析

应用场景

存内搜索TCAM、AI推理、低功耗存内计算