WaytoICT › 香农学术库 › IEDM 2025 › 论文

采用β-W电极与初始固相外延的HZO MFM:厚度≤3nm下创纪录45μC/cm2的2Pr、创纪录60的2Pr/Vop与>8E12耐久,并用于1.2V NVSRAM

HZO MFM with Record 45μC/cm2 2Pr @ ≤3nm, Record 60 2Pr/Vop, and Record >8E12 Endurance by β-W Electrodes and Initial Solid Phase Epitaxy with 1.2V NVSRAM Applications
新兴存储器FeRAM与FeFETMIM/MOS电容铁电HZO硅基CMOS实验
IEDM 2025台湾大学
用β-W电极、水淬火与初始固相外延做出3nm HZO MFM,2Pr达45μC/cm2、耐久超8E12次,并集成1.2V NVSRAM。

基本信息

作者
Yu-Tsung Liao1,+, Jhih-Yuan Liang2,+, Tao Chou2, Guan-Hua Chen1, Yun-Wen Chen1, Yu-Rui Chen1, Wei-Jen Chen1, Min-Kuan Lin2, Yan-Jyun Chen1, Yu-An Chen1, Bo-Hui Yu3, Hidenari Fujiwara1, Ming-Chang Liu1, Kuan-Heng Lin1, Dai-Ying Lee4, Ming-Hsiu Lee4, and C. W. Liu1,2,3,*
机构
台湾大学
国家
中国台湾
会议
IEDM 2025(International Electron Devices Meeting)
工艺节点
0.18μm SRAM 单元(6T2C NVSRAM);MFM 铁电层 3nm/3.5nm HZO
供电电压
0.75V(主回线工作电压)、0.55V(低压工作)、1.2V(NVSRAM store/recall)
电路架构
6T2C NVSRAM(0.18μm 6T SRAM 单元 + 两个 BEOL 外置 MFM FeCAP,共享板线 PL)

摘要

采用水淬火与H2等离子体处理抑制β-W电极向HZO扩散,使3nm HZO金属-铁电-金属(MFM)电容的漏电流(+0.75V下2.6E-2 A/cm2)降低4个数量级。初始固相外延(ISPE)使剩余极化(2Pr)提升40%,在厚度≤3nm时实现创纪录的45μC/cm2 2Pr,并获得所有MFM中创纪录的60的2Pr/Vop比。在0.75V主回线工作电压下,3nm HZO电容实现超过8E12次循环的创纪录无疲劳耐久性,最终2Pr仍为45μC/cm2。即使在0.55V更低工作电压下,经8E12次循环后仍保持29μC/cm2的2Pr,高于2023 IRDS目标。具有1.4V低矫顽电压(2Vc)和27μC/cm2 2Pr的3.5nm HZO MFM电容被集成到非易失SRAM(NVSRAM)单元中。在1.2V存储电压下,可靠的非易失召回电压低至1.2V。

Abstract

The leakage current (2.6E-2A/cm2@+0.75V) of 3nm HZO metal-ferroelectric-metal (MFM) capacitor is reduced by 4 orders of magnitude using water quenching and H2 plasma due to the diffusion suppression of β-W electrode into HZO. Initial solid phase epitaxy (ISPE) enhances remanent polarization (2Pr) by 40%, achieving record high 2Pr of 45μC/cm2 for the thickness ≤3nm and record high 2Pr/Vop ratio of 60 among all MFMs. At 0.75V operating voltage for major loops, the 3nm HZO capacitor achieves record fatigue-free endurance exceeding 8E12 cycles with final 2Pr of 45μC/cm2. Even at lower Vop of 0.55V, 2Pr of 29μC/cm2 larger than the 2023 IRDS target is maintained after 8E12 cycle endurance. 3.5nm HZO MFM capacitors with low coercive voltage (2Vc) of 1.4V and 2Pr of 27μC/cm2 are integrated into non-volatile SRAM (NVSRAM) cells. The reliable non-volatile recall voltage is as low as 1.2V with the store voltage of 1.2V.

关键技术指标

指标数值说明
剩余极化 2Pr45 μC/cm23nm HZO 加 ISPE 在 0.75V 工作电压下,为 ≤3nm 厚度最高纪录
2Pr/Vop 比60 (45/0.75)所有 MFM 中最高,源于 HZO 厚度减薄使工作电压降低
耐久性>8E12 次循环0.75V 下无疲劳、无击穿,末态 2Pr 仍为 45 μC/cm2
漏电流2.6E-2 A/cm2 @+0.75V水淬火+ H2 等离子体抑制 W 扩散后降低约 4 个数量级
低压 2Pr29 μC/cm2 @0.55V经 8E12 次循环后仍超过 2023 IRDS 目标 26.5 μC/cm2
3.5nm HZO 电容/NVSRAM2Vc = 1.4V,2Pr = 27 μC/cm2集成入 6T2C NVSRAM,store 与 recall 均可在 1.2V 完成

性能概述

2Pr = 45 μC/cm2 @ ≤3nm(0.75V);耐久 >8E12 次循环无疲劳

技术路线

铁电极化、外延生长

应用场景

嵌入式非易失存储、非易失SRAM(NVSRAM)、先进逻辑CMOS后端集成

打开交互版 · AI 解读 / 同类对比 / 完整指标在香农学术库中查看(需会员)

同领域论文

← 返回香农学术库
蜀ICP备2020035321号-2