WaytoICT › 香农学术库 › IEDM 2025 › 论文

亚10 nm全原子层沉积MFM堆叠及可靠性增强:3 nm铁电HZO中创纪录低漏电与创纪录高击穿场强

Sub-10 nm Fully Atomic-Layer-Deposited MFM Stack with Enhanced Reliability: Record-low Ileakage and Record-high EBD in 3 nm Ferroelectric HZO
新兴存储器FeRAM与FeFETMIM/MOS电容铁电HZO实验+仿真
IEDM 2025National University of Singapore
9 nm全ALD MFM堆叠,3 nm HZO实现低漏电、高击穿场和超10^11次耐久。

基本信息

作者
Xiaolin Wang1*, Yang Feng1,2*, Yaoyu He2, Yuye Kang1, Jixuan Wu2, Wei Shi1, Jiawei Xie1, Zhilun Zhang1, Zijie Zheng1, Leming Jiao1, Zuopu Zhou1, Dong Zhang1, Chen Sun1, Gan Liu1, Gengchiau Liang1,3, Jiezhi Chen2# and Xiao Gong1,4#
机构
National University of Singapore
国家
新加坡
会议
IEDM 2025(International Electron Devices Meeting)
工艺节点
3 nm HZO(铁电层厚度节点)
供电电压
2Vc <0.65 V(矫顽电压)
电路架构
5 μm×5 μm crossbar结构MFM电容器

摘要

我们展示了全原子层沉积(ALD)的金属-铁电-金属(MFM)电容器,其总厚度最小为9 nm(3 nm TiN/3 nm HZO/3 nm TiN)。我们的超薄器件不仅实现了创纪录低的矫顽电压(2Vc <0.65 V),还在3 nm铁电(FE)层的多项关键可靠性指标上设立了新基准:超低漏电流密度(3 MV/cm下<10^-3 A/cm2)、超高击穿电场(EBD超过9.5 MV/cm),以及超过10^11次循环且无铁电失效的优异耐久性(最终2Pr >18 μC/cm²且无电击穿)。我们全面的表征和分析表明,这些突破源于将TiN电极减薄至8 nm以下所释放的两个关键性能提升优势:(1)TiN从多晶向非晶的转变促进HZO中o相形成,使HZO和TiN层可同时按比例缩小;(2)更光滑的TiN表面和受抑制的氧清除共同降低了漏电流并提高了击穿强度。我们的发现凸显了全ALD生长的TiN/HZO/TiN堆叠优异的厚度可缩放性和出色性能,为3D集成超高密度FE存储器提供了一条有前景的路径。

Abstract

We demonstrate fully ALD-deposited metal-ferroelectric-metal (MFM) capacitors featuring the smallest total thickness of 9 nm (3 nm TiN/3 nm HZO/3 nm TiN). Our ultra-thin devices not only achieve a record-low coercive voltage (2Vc <0.65 V), but also set new benchmarks in several key reliability metrics for 3 nm ferroelectric (FE) layers: an ultralow leakage current density (<10^-3 A/cm2 at 3 MV/cm), an ultrahigh breakdown electric field (EBD) exceeding 9.5 MV/cm, and exceptional endurance exceeding 10^11 cycles without ferroelectricity failure (final 2Pr >18 μC/cm² and no electrical breakdown). Our comprehensive characterization and analysis reveal that these breakthroughs are driven by two critical performance-enhancing benefits unlocked by thinning TiN electrodes below 8 nm: (1) the transition from polycrystalline to amorphous TiN promotes o-phase formation in HZO, allowing simultaneous downscaling of both HZO and TiN layers; and (2) smoother TiN surfaces and suppressed oxygen scavenging collectively minimize leakage current and enhance breakdown strength. Our findings highlight the superior thickness scalability and outstanding performance of fully ALD-grown TiN/HZO/TiN stacks, offering a promising pathway toward 3D-integrated, ultra-high-density FE memories.

关键技术指标

指标数值说明
总堆叠厚度9 nm3 nm TiN/3 nm HZO/3 nm TiN,为已报道最小总厚度MFM堆叠
矫顽电压2Vc <0.65 V超薄MFM器件实现创纪录低矫顽电压
漏电流密度<10^-3 A/cm2 @3 MV/cm3 nm HZO铁电层在3 MV/cm下的超低漏电
击穿电场>9.5 MV/cm3 nm HZO实现超高EBD
耐久性>10^11 cycles无铁电失效且无电击穿,最终2Pr >18 μC/cm²
剩余极化2Pr >22 μC/cm²3 nm HZO夹在3 nm TiN电极间仍保持强铁电性

性能概述

漏电流密度 <10^-3 A/cm2 @3 MV/cm;击穿电场 EBD >9.5 MV/cm

技术路线

原子层沉积(ALD)、铁电极化、TDDB、失效分析

应用场景

3D DRAM、超高密度铁电存储器、低功耗存储器

打开交互版 · AI 解读 / 同类对比 / 完整指标在香农学术库中查看(需会员)

同领域论文

← 返回香农学术库
蜀ICP备2020035321号-2