WaytoICT › 香农学术库 › IEDM 2025 › 论文

具有超薄IGZO电荷陷阱层的高可靠铁电NAND单元:面向耐久性与保持特性改善的陷阱分布调控

A Highly Reliable Ferroelectric NAND Cell with Ultrathin IGZO Charge Trap Layer: Trap Profile Engineering for Endurance and Retention Improvement
新兴存储器FeRAM与FeFET3D NANDFeFET氧化物半导体(IGZO/ITO)实验
IEDM 2025Korea Advanced Institute of Science and Technology
在FeNAND栅栈中插入2 nm IGZO电荷陷阱层并原位N2掺杂调控陷阱能级,实现9.4 V窗口、10年TLC保持与超80k次擦写。

基本信息

作者
Hyunjun Kang1*, Hongrae Joh1*, Junhyeok Kwak1, Giuk Kim1, Hyojun Choi1, Hoon Kim1, Sanghyun Park2, Kwangyou Seo2, Kwangsoo Kim2, Wanki Kim2, Daewon Ha2, Jinho Ahn3+, and Sanghun Jeon1+
机构
Korea Advanced Institute of Science and Technology
国家
韩国
会议
IEDM 2025(International Electron Devices Meeting)
供电电压
工作电压 VOP < 17 V(栅极偏置 ±3 V 用于能带弯曲电荷损失测试)

摘要

我们展示了一种具有经工程化设计的InGaZnO(IGZO)电荷陷阱层(CTL)的铁电NAND(FeNAND)单元,用于可靠的三维集成。为克服传统金属栅-界面层(G.IL)-铁电(FE)-沟道界面层(Ch.IL)-Si(MIFIS)栅栈中存在的耐久性退化以及保持(retention)过程中严重的存储窗口(MW)损失,我们提出了一种引入2 nm厚IGZO CTL的金属-G.IL-氧化物半导体(OS)-FE-Ch.IL-Si(MISFIS)结构。该IGZO CTL同时充当氧储层以抑制FE层中氧空位(VO)的形成,并提供能带偏移以减少电荷损失。采用原位N2掺杂来调控陷阱分布,在2 sccm流量下获得以深能级为主的陷阱。这一优化设计实现了9.4 V的宽存储窗口、低于17 V的低工作电压(VOP)、超过10年的稳定三值单元(TLC)保持特性,以及超过80k次编程/擦除(PGM/ERS)循环的稳健耐久性。这些结果验证了MISFIS FeNAND作为下一代三维铁电存储器颇具前景的架构。

Abstract

We demonstrate a ferroelectric NAND (FeNAND) cell featuring an engineered InGaZnO (IGZO) charge trap layer (CTL) for reliable 3D integration. To overcome endurance degradation and severe memory window (MW) loss during retention in conventional metal-gate interlayer (G.IL)-ferroelectric (FE)-channel interlayer (Ch.IL)-Si (MIFIS) gate stacks, we propose a metal-G.IL-oxide semiconductor (OS)-FE-Ch.IL-Si (MISFIS) structure incorporating a 2 nm-thick IGZO CTL. The IGZO CTL simultaneously serves as an oxygen reservoir to suppress oxygen vacancy (VO) formation in the FE layer and provides an energy band offset to reduce charge loss. In-situ N2 doping is applied to tailor the trap profile, achieving deep-level dominant traps at a 2 sccm flow rate. This optimized design enables a wide MW of 9.4 V with a low operation voltage (VOP) below 17 V, stable triple-level cell (TLC) retention over 10 years, and robust endurance exceeding 80k program/erase (PGM/ERS) cycles. These results validate the MISFIS FeNAND as a promising architecture for next-generation 3D FE memories.

关键技术指标

指标数值说明
存储窗口 (MW)9.4 V优化后(2 nm IGZO CTL + 2 sccm N2掺杂)器件的最大存储窗口,可满足TLC工作
工作电压 (VOP)< 17 V宽MW下仍保持低于17 V的低工作电压,优于传统CTF的>20 V
耐久性> 80k PGM/ERS 循环优化MISFIS单元可承受超过8万次编程/擦除循环
保持特性10年 (保持74% MW)外推10年后仍保留最大存储窗口的74%,支持TLC
IGZO CTL 厚度2 nm最优氧化物半导体厚度,兼具最宽MW与最高击穿电压
HfO2亚氧化物比例由23.2%降至7.4%XPS证实IGZO作为氧储层对HfO2的氧清除作用

性能概述

存储窗口 MW 9.4 V;耐久性 > 80k PGM/ERS 循环

技术路线

电荷俘获、铁电极化

应用场景

3D NAND闪存、高密度三维存储、AI加速器存储