在HfO2基铁电器件中,既克服极化疲劳又实现低电压工作仍是一项关键挑战。本文提出一种非对称脉冲电压工程方法,并结合界面与热预处理,在超薄Hf1-xZrxO2(HZO)电容器中同时获得抗疲劳能力与稳健的铁电性。我们的器件在1V工作下表现出超过1.2×10¹²次耐久循环(受测量时间限制),且2Pr稳定性优异(波动<5%)。此外,高温唤醒进一步提升了剩余极化(Pr),同时保持无疲劳特性。这是首次在1V下实现亚5 nm HZO的无疲劳、高耐久工作,为低功耗铁电存储器提供了一条有前景的路径。
Overcoming polarization fatigue while enabling low-voltage operation remains a key challenge in HfO2-based ferroelectric devices. Here, we introduce an asymmetric pulse voltage engineering approach, combined with interfacial and thermal preconditioning, to achieve both fatigue immunity and robust ferroelectricity in ultrathin Hf1-xZrxO2 (HZO) capacitors. Our device exhibits >1.2×1012 endurance cycles (limited by measurement time) with excellent 2Pr stability (<5% variation) under 1V operation. Moreover, high-temperature wake-up further boosts remnant polarization (Pr) while preserving fatigue-free characteristics. This represents the first demonstration of fatigue-free, high-endurance operation in sub-5 nm HZO at 1V, offering a promising pathway for lowpower ferroelectric memories.
| 指标 | 数值 | 说明 |
|---|---|---|
| 耐久性(Endurance) | >1.2×10^12 cycles | 1V工作下无疲劳循环次数,受测量时间限制 |
| 剩余极化2Pr | >17 μC/cm² | 1V操作并循环后仍保持的2Pr水平 |
| 2Pr稳定性 | 波动<5% | 整个耐久测试过程中2Pr的变化幅度 |
| 界面层厚度 | 7 Å | 插入底电极与HZO之间以稳定正交相的超薄界面层 |
| HZO薄膜厚度 | 4.5 nm | 亚5 nm超薄HZO铁电层 |
| 2Pr提升(含IL对比) | 4.3 → 25.3 μC/cm² | ±2.4V、100kHz双极循环下有无界面层的对比 |
耐久性 >1.2×10^12 cycles @1V;2Pr >17 μC/cm²(波动<5%)
铁电极化、原子层沉积(ALD)、高k金属栅、热稳定性
铁电存储器(1TnC FeRAM)、低功耗嵌入式存储、先进DRAM替代
打开交互版 · AI 解读 / 同类对比 / 完整指标在香农学术库中查看(需会员)