本文通过宽温区表征系统研究了HfO2基铁电(FE)薄膜的保持特性损失。首次观察到保持损失与印记(imprint)之间存在极强的相关性,并可用温度激活的印记中心(TI)模型很好地解释。基于第一性原理计算,揭示了电荷辅助缺陷迁移与翻转(CDMS)可能是其内在机制,即印记源于Vo2+向界面的迁移,而局域退极化则由Vo2+引起的翻转势垒降低所致。为缓解该问题,提出了结合陷阱中和的缺陷工程方案(DTNS)。结果表明,通过采用工艺优化降低氧空位(Vo)并结合电子预注入中和Vo2+,可实现约28%的印记降低和约21%的保持特性提升。本工作为HfO2基铁电器件的保持特性优化策略提供了启示。
Retention loss in HfO2-based ferroelectric (FE) thin films is investigated systematically through wide-temperature characterizations. For the first time, it is observed that retention loss has an extremely strong correlation with imprint, which can be well explained by temperature-activated imprint-centric (TI) model. Based on first-principles calculations, it is revealed that charge-assisted defect migration and switching (CDMS) could be the intrinsic mechanism, that is, imprint originates from Vo2+ migration to the interface while localized depolarization is caused by Vo2+-induced switching barrier reduction. To mitigate this, a defect-engineering with trap neutralization scheme (DTNS) is proposed. It is demonstrated that, by adopting process optimization to lower Vo and electron pre-injection to neutralize Vo2+, ~28% imprint reduction and ~21% retention enhancement can be achieved. Our results shed light on retention optimization strategies in HfO2-based FE devices.
| 指标 | 数值 | 说明 |
|---|---|---|
| 印记电压降低 | ~28% | 采用工艺优化降Vo与电子预注入中和Vo2+的DTNS方案后印记改善幅度 |
| 保持特性提升 | ~21% | 同等DTNS方案下铁电电容器剩余极化保持能力的提升 |
| 热激活能 | ~0.79 eV | 由阿伦尼乌斯关系提取,与计算的Vo/Vo2+垂直迁移势垒高度吻合 |
| 保持特性测试温度区间 | 300-400 K | 宽温区保持测试与10年外推所覆盖的温度范围 |
| 保持特性测试时间 | 1-10^5 s | 幂律外推(Pr/Pr0 = t^-k)所用长时间区间的保持测试时长 |
印记电压降低约28%;保持特性提升约21%
铁电极化、电荷俘获、原子层沉积(ALD)、失效分析
嵌入式非易失存储器、铁电存储器(FERAM)、高可靠高温存储